Abstract

Novel bioactive amorphous glass-glass composite scaffolds (ICIE16/BSG) with interconnected porosity have been developed. Hierarchically interconnected porous glass scaffolds were prepared from a mixture of two melt-derived glasses: a ICIE16 glass previously developed by Wu et al. (2011) to prevent crystallization, and a borosilicate glass of composition 73.48 SiO2-11.35 B2O3-15.15 Na2O (wt%). The resulting melt derived glass-glass composite scaffolds (ICIE16/BSG) were subject to surface functionalization to further improve its biological properties. This was performed by a nitridation process with hot gas N2/ammonia at 550 °C for 2 h, obtaining the ICIE16/BSG-NITRI. Evaluation of the degradation rate and the conversion to hydroxyapatite after immersion in simulated body fluid predicted a good biological activity of all the scaffolds, but particularly of the nitrided ones. In vitro evaluation of osteoblastic cells cultured onto the nitrided and non-nitrided scaffolds showed cell attachment, proliferation and differentiation on all scaffolds, but both proliferation and differentiation were improved in the nitrided ICIE16/BSG-NITRI. Statement of significance Biomaterials are often required in the clinic to stimulate bone repair. We have developed a novel bioglass (ICIE16/SBG-NITRI) that can be sintered into highly porous 3D scaffolds, and we have further improved its bioactivity by nitridation. ICIE16/SBG-NITRI was synthesized from a mixture of two melt-derived glasses through combined gel casting and foam replication techniques, followed by nitridation. To mimic bone, it presents high-interconnected porosity while being mechanically stable. Nitridation improved its reactivity and bioactivity facilitating its resorption and the deposition of apatite (bone-like mineral) on its surface and increasing its degradation rate. The nitrided surface also improved the bioglass' interaction with bone cells, which attached and differentiated better on ICIE16/SBG-NITRI.

Description

Bibliographic citation

Collections

Endorsement

Review

Supplemented By

Referenced by

Creative Commons license

Except where otherwised noted, this item's license is described as Attribution-NonCommercial-NoDerivatives 4.0 Internacional