Clinkering of calcium sulfoaluminate clinkers: polymorphism of ye'elimite
(2018)
The manufacture of CSA cements is more environmentally friendly than that of OPC as it releases
less CO2. This reduction depends on CSA composition and is due to three factors: i) less emissions
from decarbonation in the ...
Clinkering and hydration of belite-ye'elimite-alite cement
(Elsevier, 2017)
Some belite-ye´elimite-ferrite (BYF) cements present low mechanical strengths mainly due to the slow reactivity of belite. A solution to this problem may be the activation of BYF clinkers by preparing them with a coexistence ...
Design and optimisation of new formulations of Belite-Alite Calcium Sulfoaluminate (BACSA) eco-cements
(2015-07-02)
Belite Calcium SulfoAluminate (BCSA) eco-cements were developed as OPC substitutes since in their production release 22% less CO2 than OPC. BCSA eco-cements contain belite as main phase (>50 wt%) and ye'elimite as secondary ...
Clinkering and early age hydration characterization of Belite-Alite Calcium Sulfoaluminate (BACSA) cements
(2015-10-26)
In this work, four BACSA clinkers with different compositions (belite ~ 70-55 wt %, alite ~ 10-15 wt % and ye’elimite ~ 10-15 wt %) were synthesized (at laboratory scale). Lime, gypsum, kaolin and sand were used as raw ...
Early hydration study of standard and doped Alite-Belite-Ye’elimite (ABY) cements through Synchrotron Radiation
(2018-07-09)
The manufacturing of ye'elimite-rich cements releases from 15 to 37%, depending on their
composition, less CO2 to the atmosphere than ordinary Portland cement (OPC). BYF cements
containing belite, ye’elimite and ferrite ...